Free Access

Tableau II.

Variation des propriétés mécaniques en fonction du mode de stérilisation. LCA : ligament croisé antérieur du genou.

Non stérilisé Stérilisé β Stérilisé γ
Module d’Young (MPa)

94P200 555 ± 50 452 ± 100 867 ± 27

94T200 455 ± 24,5 439 ± 48,1 656 ± 123

LCA 50-150

Contrainte à la rupture (MPa)

94P200 18,0 ± 1,6 13 ± 2,0 15,4 ± 5,8

94T200 20,0 ± 1,5 19,8 ± 3,8 16,9 ± 5,5

LCA 16-36

Allongement à la rupture (%)

94P200 600 ± 40 545 ± 200 10,3 ± 1,9

94T200 760 ± 55 965 ± 150 12,3 ± 6,0

LCA 19-36